Link to Halifax Crane Collapse - Hurr. Dorian
From CBC News
There are problems when ND testing fails to expose multiple welding defects, the crane cannot weather-vane for two weeks, follow up reports are submitted, yet the crane collapses anyway and the only penalty is a two day suspension, a $500 fine, and a conclusory note that "... the tower crane owner and operator met the applicable legislative and regulatory requirements to prevent this event from occurring" and no one picks up on the contradiction. It was only dumb luck that the crane collapsed on an unoccupied tower under construction rather than the occupied condo next door.
Toronto Star
Report from Nova Scotia Department of Labour and Advanced Education - Brenton Suites Crane Collapse
Jan 7, 2019 - was erected ... total height of approximately 73 metres (240 feet)
Jun 4, 2019 - the Safety Branch was advised by the general contractor that the turntable at the top of the tower crane had seized, preventing it from “weather-vaning” when subjected to wind loads.
Jun 17, 2019 - a new transition section (Figure 1) was installed on top of the previously erected ...
- Additionally, on this date, all the required test and certification documentation was provided to the Safety Branch, including: ... Non-destructive testing for existing tower completed in erected state
Sept 7, 2019 - at approximately 4:00 PM, the tower crane collapsed
Halifax weather history from timeanddate.com June 4, 2019 etc.
From CBC News
A welding failure is to blame for the collapse of a crane in downtown Halifax during post-tropical storm Dorian
There are problems when ND testing fails to expose multiple welding defects, the crane cannot weather-vane for two weeks, follow up reports are submitted, yet the crane collapses anyway and the only penalty is a two day suspension, a $500 fine, and a conclusory note that "... the tower crane owner and operator met the applicable legislative and regulatory requirements to prevent this event from occurring" and no one picks up on the contradiction. It was only dumb luck that the crane collapsed on an unoccupied tower under construction rather than the occupied condo next door.

Toronto Star
Report from Nova Scotia Department of Labour and Advanced Education - Brenton Suites Crane Collapse
On August 7, 2020, the metallurgical testing report for the diagonal section, node and weld was received, indicating there was a lack fusion, corrosion, pores, and a crack, which propagated from the inside diameter to the outside diameter of the area of the weld. The report also mentioned other welding defects on other welded connections.
Jan 7, 2019 - was erected ... total height of approximately 73 metres (240 feet)
Jun 4, 2019 - the Safety Branch was advised by the general contractor that the turntable at the top of the tower crane had seized, preventing it from “weather-vaning” when subjected to wind loads.
Jun 17, 2019 - a new transition section (Figure 1) was installed on top of the previously erected ...
- Additionally, on this date, all the required test and certification documentation was provided to the Safety Branch, including: ... Non-destructive testing for existing tower completed in erected state
Sept 7, 2019 - at approximately 4:00 PM, the tower crane collapsed

Halifax weather history from timeanddate.com June 4, 2019 etc.