I've got a set up to do some forming in which a piece of metal becomes a u Shape. We used to use a Galvaneal material but due to lead issues we can no longer get it. so we've been trying other materials

issues we've seen and are a little baffled by is a an .022 galvanized sheet metal and a .048 CRS form the same and as we would expect.

But a draw quality material of .048 thickness won't hold the shape and has a lot of spring back.

Just curious for a little background data on forming and the differences in draw quality material, vs CRS, vs Galvanized.

Thanks for the help!
 
Replies continue below

Recommended for you

You'll have to find out exactly what alloy and temper you got when you ordered 'draw quality'.

My guess is that maybe you got an alloy that's 'bake-hardenable', and that it's been stored in the sun.



Mike Halloran
Pembroke Pines, FL, USA
 
ns

I agree with Mike the matl is most likely work harden.
therefore more spring back.
request certs on your material, look up the data sheets, is it formable?