Hi, mates:
Have anyone any experience about chlorobenzenes fouling in chlor-alkali plants?
This used to be a problem when using graphite anodes, especially with hexachlorobenzene, but it seems not to be a common issue nowadays. But we are not using graphite anodes here and have some of these symptoms, clogging filters in the drying chlorine area. The material was analyzed, and a mixture of chlorobenzenes was found, mainly the mentioned hexachlorobenzene.
Did anyone have a similar experience? Suggestions?
Thanks
jalvarez
 
Replies continue below

Recommended for you

To jalvarez,
My experience has been in the chlorine side of plant. The valves had been known to foul with "chlorine butter" . These were changed to a globe style valve in place of the plug valves which would lock up.
The graphite rods probably have a resin binder in the matrix. I had not thought of it before, but that might be the source of hydrocarbon for making hexachlorobenzene. A different source of graphite rod might reduce resin content. Sorry I can't be more helpful.
 