We are currently using a galvaneal product that is us weld quality issues...ie: porosity, lack of fussion.
The above mentioned material is domestically manufactured. We are also using an import material for a similar product. This material provides no weld issues.
We have been told that no one in the United States can produce this material coating @ 45grams/m squared with complete coverage.
Can anyone confirm this, or...if you no of a manufacturer, could you please provide me with the contact.
Thanks