I am doing deflection analysis of a pipe using GRE (Glass reinforced epoxy) pipe for which i ahve the following properties @ 21 Deg. C from material supplier
Hoop Tensile modulus = 23250 MPa
Poisson's ratio axial/hoop = 0.93
Axial Tensile Modulus = 10000 MPa
Poisson's ratio hoop/axial = 0.40
In FEA when i enter the poisson's ratios i get a message that the values ae not practical or with these values strain energy will be negative. I am using transvere isotropic format for GRE in FEA.
Will you suggest me on how to correct the problem of poissonss ratio.
I am doing deflection analysis of a pipe using GRE (Glass reinforced epoxy) pipe for which i ahve the following properties @ 21 Deg. C from material supplier
Hoop Tensile modulus = 23250 MPa
Poisson's ratio axial/hoop = 0.93
Axial Tensile Modulus = 10000 MPa
Poisson's ratio hoop/axial = 0.40
In FEA when i enter the poisson's ratios i get a message that the values ae not practical or with these values strain energy will be negative. I am using transvere isotropic format for GRE in FEA.
Will you suggest me on how to correct the problem of poissonss ratio.