Hi guys, I've been through some welding spec for piping/pressure vessels and was curious about one requirement:
GMAW may be used for fill passes provided the transfer mode is globular or spray arc and the completed thickness is of the weld is no greater than 9.5 mm.
Does anybody know what can be the reason for that? Is it due to reliability (defect rate) of GMAW?
GMAW may be used for fill passes provided the transfer mode is globular or spray arc and the completed thickness is of the weld is no greater than 9.5 mm.
Does anybody know what can be the reason for that? Is it due to reliability (defect rate) of GMAW?