I have a section of In725 that appears to have a nearly continuous carbide network at the grain boundaries.
Is this typical for this grade?
Heat treatment was:-
1040c for 11hr/air cool
730c for 12hr/furnace cool to 620c hold for 8hr/air cool
Hardness 37HRC
Thanks in advance.