Hi,
Is there anyone running the Gweike LF3015GA fiber laser? If so, is it good laser and operate easily?
 
Replies continue below

Recommended for you

Hi,

yes, we have this laser machine from Czech dealer and it is just fine. Fiber laser with easy oparations. I can recommend this cutting CNC laser.

Have a nice day.

Greetings from Czech Republic.
 
@Kovo drs
Do you know how to cut with fixed height hold (the laser won’t move up and down)? We want to cut something not flat so we want to keep the head not move up down to avoid crashing the head.
 