I have a stana=dard product which is made from Mild steel. I currently have an application where this componenet will be placed in an environment where H2S will be present. Would it be better to epoxy the componenet or use a differnet material?
 
Replies continue below

Recommended for you

A-560 Corten B would be a good material to use. It has the same weldability as carbon steel. In simple terms it is carbon steel with some copper tossed in. This has been used on chimneys for some time.
 