We have an Amada F0 3015 Laser and we have issues with the second half of the sheet, with Aluminum the cut starts to blister up and wont cut at all, with steel it appears to cut but the bottom welds its self together. we have had Amada techs tell us it was a problem coming from the resinator so they messed with that and the problem is still there . they have come out to clean our mirrors and nothing changes finally we have replaced all internal mirrors and external mirrors and the problem is still there but it comes and goes sometimes we cut great and other times we cant cut anything, has any body had this problem with any laser? if so how did you fix it??? Thanks Alot we have no one to turn to not even Amada!!