Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations pierreick on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Help ! can some one help identify this !!!

Status
Not open for further replies.

geno22

Geotechnical
Aug 17, 2011
1
I found this material on my land and i would like to find a use for it. It is magnetic and heavy (in the iron family ) it doesn't seem to rust though. I had 2 pieces analyzed and they came back, the first

1) 73% fe, <0.003 C and the remainder is oxygen other metals ARE MANGANESE .43 silicon .76 al .65 the res is trace amounts.

the second 2) fe 65% .001 C, MANGANESE.34 silicon 2.6 al 3.08 titanium .24 the rem is oxygen

I would like to sell this if i can ,and i would really like to know what it is. I can also upload the analysis sheet if necessary.
thanks in advance
Geno

pictures


 
Replies continue below

Recommended for you

Looks like iron ore. Use it for landscape rock.
 
You named the pics Ore1, Ore2. hmm.

65% and 73% Fe. That has to be iron ore. [smile]


[peace]
Fe
 