meps11
Materials
- Nov 4, 2016
- 35
Hi all I cut is gal and been using MS condition settings using 7.5 lens and 1.7 nozzle with shop air or N2 any one cutting 10 gauge MS if so can you tell me what your settings are? Using a Mitsubishi 3015 no conditions in the machine for 10 gauge go everything else. been playing with the focus or gap and doesn't seem to be getting any ware THX