Hi,
I need to clarify with my supplier that they disagree with my point of view on the interpretation of ASME section VIII div. 1 UG-84(h)(3). The PQR is made on a 1 1/2 inch plate to be welded on both sides with a CVN requirement.
My point of view is that UG-84 (h) (3) is this: Material Over 1 1/2 in. is T > or = at 1 1/2 in. and not T > 1 1/2 in.
So for 1 1/2 in. test coupon we need 2 set of charpy in the weld and 2 set in th HAZ.
Do you agree?
I need to clarify with my supplier that they disagree with my point of view on the interpretation of ASME section VIII div. 1 UG-84(h)(3). The PQR is made on a 1 1/2 inch plate to be welded on both sides with a CVN requirement.
My point of view is that UG-84 (h) (3) is this: Material Over 1 1/2 in. is T > or = at 1 1/2 in. and not T > 1 1/2 in.
So for 1 1/2 in. test coupon we need 2 set of charpy in the weld and 2 set in th HAZ.
Do you agree?