I am in the UK and would like to find a source of steel with a expansion coefficient in the region of 20?m/m.°C, preferably in plate form (although larger section bar, which could be forged flat could be acceptable).At the moment we are using austenitic stainless, but ideally need to increase the expansion.
Our primary supplier of metal cannot get hold of AMS 5623 and the lead time on Aubert & Duval's GD223 is too long.
I would appreciate any advice on alternative steels with expansion coefficients around this value or possible suppliers I could try.
Thank you in advance.
Our primary supplier of metal cannot get hold of AMS 5623 and the lead time on Aubert & Duval's GD223 is too long.
I would appreciate any advice on alternative steels with expansion coefficients around this value or possible suppliers I could try.