Hi everyone, I'm hoping somebody out there can help me. Does anyone know where can I find High Temperature Solder that can withstand at least 800 degrees celsius. I would greatly appreciate the assisstance!
I guess that this isn't for soldering electronic parts. Soldering at these temperatures is called brazing. Google this word and you will find lots of data on it.
For these temperatures I think you would braze or weld (cap discharge welder). However, I do remember that there are some indium solders that are high temp, and a quick search found this chart that has solders up to 1064 C !