Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

High Temperature Galvanized Coating Options

Status
Not open for further replies.

schulkfl

Mechanical
Jan 31, 2008
10
US
I currently have a unit that is made of zinc-coated mill galvanized steel. It is my understanding that reaching temperatures above 230°C will cause the metal to flake and compromise the mechanical properties.
Are there cost effective alternatives that will allow us to reach ~300°C without having these issues (for example, other coatings)? The material or coating must be corrosion resistant as the unit is outdoor.


Thanks in advance for any help-

Fred S
 
Replies continue below

Recommended for you

Aluminized steel works to higher temps than 300 [°]C.
 