What kind of aluminium alloy grade that has the highest UTS for temperature up to 300° celsius?
 
Replies continue below

Recommended for you

But why? Latent heat of aluminum is so high as it is, and the conductivity is so high... why would you choose aluminum? You could likely add cooling to your part.

Otherwise time to look at titanium. Aluminum isn't a hot working material.

 