I recently got a call from a steel fabricator regarding some oversized holes we had specified.
The bolts in question are 1" diameter A490 SC bolts in oversized holes through 1.25" thick plate. The fab said that he wanted to use bigger holes than 1.25" because of his punching machine.
The code has maximum hole dimensions published in table J3.3, but what are the problems with the use of say a 1-5/16" hole as opposed to a 1.25" hole for a SC connection with 1" bolts in OVS holes.
He is proposing to use 1-1/8" bolts instead of 1" bolts to work with his shops limitations. Has anyone else run into such a problem before?
I recently got a call from a steel fabricator regarding some oversized holes we had specified.
The bolts in question are 1" diameter A490 SC bolts in oversized holes through 1.25" thick plate. The fab said that he wanted to use bigger holes than 1.25" because of his punching machine.
The code has maximum hole dimensions published in table J3.3, but what are the problems with the use of say a 1-5/16" hole as opposed to a 1.25" hole for a SC connection with 1" bolts in OVS holes.
He is proposing to use 1-1/8" bolts instead of 1" bolts to work with his shops limitations. Has anyone else run into such a problem before?