Has anyone encountered horizontal cracks in beam right below the slabs just like in the picture above? What could have caused it?
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
the cause could be that the slab does not deform simultaneously with the beam producing to much compressive stress in the slab that the stirrups (acting as shear studs) are insufficient to resist the shear stress being produced between the junction of the slab and the beam.