CoFe2

Industrial
Sep 20, 2018
7
Wondering if anyone has some knowledge on additional requirements for hot forming elliptical heads made from SB-443 N06625 Inconel, as far as post forming annealing or heat treat when building to ASME Section VIII. I have looked around material specs and Section VIII but only find requirements for Carbon steels and ferritic steels but nothing on high nickel alloys.

Thanks!
 
Replies continue below

Recommended for you

Chrisbnwc, if this is Div 1 work, see UNF-79

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
It is Div 1. Thanks for the direction!
 
Certainly & good luck :)