Hi everyone
I have question about pipe wall thickness under external pressure condition.
I know it can be calculated in accordance with ASME BPVC SEC VIII - UG 28.
In this code, I must determine factor "A" and "B", and it can be determined in ASME SECTION II -1.
But, sometimes I cannot determined factors because Do/t or L/Do do not exist in the table G (in the ASME SECTION II- Subpart 3)
In this situation, what is the best way to determine the factor A & B?
Plz, help me.
Best regards, Moong.
I have question about pipe wall thickness under external pressure condition.
I know it can be calculated in accordance with ASME BPVC SEC VIII - UG 28.
In this code, I must determine factor "A" and "B", and it can be determined in ASME SECTION II -1.
But, sometimes I cannot determined factors because Do/t or L/Do do not exist in the table G (in the ASME SECTION II- Subpart 3)
In this situation, what is the best way to determine the factor A & B?
Plz, help me.
Best regards, Moong.