Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How long can form oil last on forms?

Status
Not open for further replies.

Hoboneer

Structural
Sep 19, 2016
17
So the contractor built the form but is unable to pour for a while due to some unforseen conditions. Is there a code stipulation as to how long the form release agent can be on the forms before pouring the concrete?
 
Replies continue below

Recommended for you

I would defer to the manufacturer's recommendations.
 
Are you talking a day or two or a week or two? After a couple of days, I would be looking at the supplier's data sheet.

Dik
 
depends on the form material and weather..
If wood, won't last long...a few days at most. if humidity is low....less because the form oil soaks more into wood
If steel, will last a lot longer.

As others note, check manufacturer's info. Will also depend on whether release agent is petroleum based or polymer based
 
...and when you find splinters of plywood adhered to the concrete, you know it was too long.