ISO 4990-2023
6.2.2.1 Test blocks
The test blocks may be cast separately, attached to the castings or cast integrally on the castings.
Unquote
How to define and interpret the three test block types?
We have tried to give an explanation of the three types of test blocks, but we don't know if it is correct.
cast separately: Test blocks cast in a separate sand mould under representative manufacturing conditions and material.
attached to the castings:Test blocks attached directly to the casting.
cast integrally on the castings:test specimen cut from casting
Your promote reply will be greatly appreciated.
Thank you.
ISO 4990-2023
6.2.2.1 Test blocks
The test blocks may be cast separately, attached to the castings or cast integrally on the castings.
Unquote
How to define and interpret the three test block types?
We have tried to give an explanation of the three types of test blocks, but we don't know if it is correct.
cast separately: Test blocks cast in a separate sand mould under representative manufacturing conditions and material.
attached to the castings:Test blocks attached directly to the casting.
cast integrally on the castings:test specimen cut from casting
Your promote reply will be greatly appreciated.