CSunny
Mechanical
- Jun 1, 2022
- 21
I am having some confusion if the material I have is 316 or 316l. This is a SA-249 Stainless steel tube. Based on the material composition and strength requirements, the material fall into both.
If I consider the tube as 316, I could use the HA2 chart for external pressure and the required thickness for the tube will be less than the HA4 chart for 316L. So, how should i approach it?
C Mn P S Si Ni Cr Mo Ti
Actual Tube 0.029 1.43 0.026 0.018 0.41 10.18 16.25 2.1 -
If I consider the tube as 316, I could use the HA2 chart for external pressure and the required thickness for the tube will be less than the HA4 chart for 316L. So, how should i approach it?
C Mn P S Si Ni Cr Mo Ti
Actual Tube 0.029 1.43 0.026 0.018 0.41 10.18 16.25 2.1 -