Hi,
i have the following connection which is RHS250x150x12.5(beam) directly welded (CJP) to SHS180x180x12.5 / SHS150x150x12.5(column), the angle was provided as a seat and it was supposed to be removed after welding three sides of the beam then weld the lower side.
Now i have been told that the angles have been welded 8 or 10 mm (to the column) by mistake and they CAN'T remove it ! is that acceptable ? what should i do as a recovery and how can i check it ?
i have the following connection which is RHS250x150x12.5(beam) directly welded (CJP) to SHS180x180x12.5 / SHS150x150x12.5(column), the angle was provided as a seat and it was supposed to be removed after welding three sides of the beam then weld the lower side.
Now i have been told that the angles have been welded 8 or 10 mm (to the column) by mistake and they CAN'T remove it ! is that acceptable ? what should i do as a recovery and how can i check it ?