Lnewqban
Mechanical
- Nov 1, 2013
- 85
“There was a motorist, one individual on a motorcycle and one individual in a car, that were proceeding west-bound on I-20 when they saw the buckled road,..........But it was too late for them to avert it so they actually went up the broken-up concrete in an upward fashion — as if they were going up in a jump.”
![URL]](https://res.cloudinary.com/engtips/image/fetch/w_800,c_lfill,q_auto,f_auto,g_faces:center/[URL unfurl="true"]http://cbsnews3.cbsistatic.com/hub/i/r/2017/04/18/2a43a730-eff2-452b-97b3-bccb1a5fd3b3/thumbnail/620x350/8dd8c23b469ad75d5fae00039bfd56d8/screen-shot-2017-04-18-at-11-16-08-am.png[/URL])
"Where the spirit does not work with the hand, there is no art." - Leonardo da Vinci