I am a qc inspector(beginner) how can I identify the solid bar( 4130) can be used for manufacturing api 16 A/6 A product from mill heat certificate. Can any one explain the method???
 
Replies continue below

Recommended for you

You have the solid bar and you're trying to confirm that it is in fact the piece that the mill cert applies to?
Or you have the solid bar and you're trying to confirm that it is in fact 4130?
Or you're trying to confirm that 4130 can be used for manufacturing your product?
For the first two questions, there should be some kind of marking (stenciling, stamping) or tagging on the material itself. Some, maybe all, of the steel standards will specify how a piece is to be marked. Your QC program should address how markings are transferred.
If it's unmarked, some standards may have provision for using material of unknown source- check the standard and see. For a small amount of material, it likely wouldn't be worth bothering with.
 
Dear Prasenjith,

The heat number will be punched on the solid bar as well as other things like the specification etc. Match the heat number with the MTC.