Materials
Jul 21, 2012
2
I am trying to possibly identify a piece of metal that I have. Its is a rectangular piece that is 31.73mm x 72.81mm x 27mm
it weighs 526 grams.
is there any way to determine what the composition is assuming that it is not an alloy and is only made of one type of metal. It does not mar easily. Any help would be greatly appreciated
 
Replies continue below

Recommended for you

Find the density and compare your value with that of known metals. But I strongly feel that this is not a professional question.

_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
 
From my calculations the density would be 8.433. Does this sound correct? From what I can determine it's most likely Brass or copper. Does this sound right?
 
Eureka!! It is Brass!

_____________________________________