Identifying wet pavement subgrades through nondestructive techniques 1

Status
Not open for further replies.

jenduro

Geotechnical
Nov 7, 2005
5
Does anybody know the best method for identifying wet soils beneath existing pavements? I have heard of using GPR, but does it work well where clays are present. Also, what about infrared imaging. Is this possible?
 
Replies continue below

Recommended for you

I don't know about non-destructive, but it wouldn't take 'much' destruction to get a core sample, and check the moisture content. You could do it with a masonry bit to get through the pavement, and then a wood auger bit to bring tailings to the surface. It wouldn't take more than a 1" hole, and you could use a hand drill (but probably not cordless.)
 
GPR does not work well for that. Infrared thermography will work on relatively thin pavements.
 