jawdayub1
Industrial
- Feb 20, 2021
- 7
Hello,
I'm looking to build olympic barbell, i have purchased 4140 grade in annealed form which typical hardness is around 20HRC. I have done knurling on the shaft but i need to increase the tensile strength. the typical tempering and hardness seems to be very expensive to meet the tensile requirements i need it at 205,000PSI. Can i do induction hardness instead? Does induction hardness increase the tensile strength of the bar. We don't have shot peen equipment where i live. How should i meet the UTS with minimum cost?
I'm looking to build olympic barbell, i have purchased 4140 grade in annealed form which typical hardness is around 20HRC. I have done knurling on the shaft but i need to increase the tensile strength. the typical tempering and hardness seems to be very expensive to meet the tensile requirements i need it at 205,000PSI. Can i do induction hardness instead? Does induction hardness increase the tensile strength of the bar. We don't have shot peen equipment where i live. How should i meet the UTS with minimum cost?