May 21, 2012 #1 Makun Mechanical Jul 20, 2009 57 0 6 AR Hi! Which is the best practice for inspection pressure vessels with internal lining? Do you have any recommended bibliography?
Hi! Which is the best practice for inspection pressure vessels with internal lining? Do you have any recommended bibliography?
May 21, 2012 #2 stanweld Materials May 9, 2003 2,906 0 0 US If paint type lining, holiday testing, dry film thickness testing and visual testing as a minimum should be required for finished coating. You need to define type of coating; i.e., paint type, elastomeric, alloy clad, weld overlay, etc. Upvote 0 Downvote
If paint type lining, holiday testing, dry film thickness testing and visual testing as a minimum should be required for finished coating. You need to define type of coating; i.e., paint type, elastomeric, alloy clad, weld overlay, etc.
May 21, 2012 Thread starter #3 Makun Mechanical Jul 20, 2009 57 0 6 AR Is there some efective method to be applied in service? Upvote 0 Downvote
May 25, 2012 #4 rustbuster Petroleum Jul 7, 1999 289 0 0 Many, what type of lining and what are you looking to find with your inspection? Upvote 0 Downvote
May 28, 2012 Thread starter #5 Makun Mechanical Jul 20, 2009 57 0 6 AR The kind of Coating is Epoxy , I want to verify the integrity of the coating and find corrosion zones Upvote 0 Downvote
The kind of Coating is Epoxy , I want to verify the integrity of the coating and find corrosion zones
May 28, 2012 1 #6 rustbuster Petroleum Jul 7, 1999 289 0 0 This would require internal inspection and Holiday testing. Upvote 0 Downvote