hardikmpanchal
Mechanical
- Jul 8, 2013
- 3
- 0
- 0
5One of Vendor has offered SS316 internal pipes for mixed bed exchanger. I m worried with its competibility with HCL. Will it be accepted? Can anyone please help me out.....
Thankyou in advance