I am designing a house with a flat roof, sloped ceiling (so the ceiling is attached to the roof joists).
The span is 19'. From IRC table 802.5.1 I can use SP #2 2x12 @ 24" O.C.
When I calculate the stress of a Southern Pine (2-4" thick, 12" wide) 2x12, repetative factor, 40 lbs dead and 40 lbs live, I get overstressed 122%
Is there something I am doing wrong? Or has the IRC just allowed roof trusses to be overstressed because they probaly will never see 20 PSF?