is f6nm steel brittle or ductile material?
 
Replies continue below

Recommended for you

At what C level? What strength? What temperature?
In general this a fairly tough material but it has its limits.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
It will be somewhere in between; precisely where depends on the quality and the heat treat condition.
No metallic alloy is truly 'brittle', metals just have varying degrees of ductility.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 