Is there someone familar to the Spec. SA-52 smls pipe? I can't find it

Status
Not open for further replies.

ZHWIL28

Mechanical
Jun 13, 2003
20
CA
Is there someone familar to the Spec. SA-52 smls pipe? I can't find it. Thanks!
 
Replies continue below

Recommended for you

2H, Are you absolutely sure you have the proper specification number? Is this a US or Overseas spec.? Never heard of SA-52, A-53 yes, but not A-52.

Sorry I couldn't be of more help.
saxon
 
I also doubt it as it appears at the material list of vendor drawing. I could not find it in ASTM or ASME.

any other ideas?
 
ZHWIL28,

I have looked at my ASTM part 1 (ferrous metals) books from 1944 to 1958, and A 52 is not part of this standard. Hope that helps.