Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

It is enough to check a material certificate according to NACEif you don't have it mentioned? 1

Status
Not open for further replies.

DeliaBoboi

Petroleum
Joined
May 27, 2013
Messages
3
Location
GB
Hello,

I am checking the material certificates for some topside application parts.
Some have the NACE standard mentioned on it, some don't.
I checked the ones that don't with the NACE standard, and they seem to comply, but is this enough?

Delia Boboi
 
Seem to comply - with what? Is this enough - what requirements does your project set? Is NACE a requirement? If so, did yopu (and how!) specify this to the supplier
How did you order the materials? If you require gold, but order rubber, you're the one to blame, not the supplier.
Too little info here.
 
The parts are on stock, they are not destined to a project. At least not yet.
The standard requirement includes NACE, but this is missing from the certificate.


Thus is the background.
 
As far as I know, as long as you verify that the material complies with MR01-75, there is no requirement that a reference to NACE be on the MTR.
 
Is it carbon steel parts that mention NACE, while 316 stainless steel parts do not?
 
No, both of them are not mentioning NACE.
 
Since the end user is responsible for ensuring that the environmental conditions are suitable for the material, and the manufacturer has no control over the environmental restrictions that ISO 15156 imposes on materials, it is not possible for a manufacturer to "certify to NACE." It is for the end user to check the inspection documents and confirm that the materials requirements for the envisaged environmental exposure have been satisfied, which is what appears to have been done in this case.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top