Need to select junction box material that withstands high temperature (to be installed in hot area, near turbine enclosure), what would be the best JB material ? JB should also have other features e.g. rigid, durable, corrosion resistant etc.

what about terminal strips/blocks inside junction box , what material is available that withstands high temperature ?

Thank you for your comments
 
Nothing about what you have described presents as a challenging environment. Painted steel or stainless steel enclosures with standard screw terminal type strips will all be sufficient. Your environment sounds hot and dry which eliminates many challenges. You may want to consider vibration isolators.
 