Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Large Diameter super-duplex heads.

Status
Not open for further replies.

vesselfab

Mechanical
Aug 21, 2007
792
I have a need for some large diameter super duplex head that will have to be manufactured in two (2)welded together prior to forming. Our suppliers here can not get the plates to quenching fast enough after annealing so the welds will be crack sensitive. Where do you guys buy these large diameter 120" to 156" i.d. 2:1 elliptical.
 
Replies continue below

Recommended for you

none of these can do it

we have gone to anonius in the netherlands

and brighton with an alternate of AL6XN
 
Did you try Europe ( France, Italy, Spain, Belgium) for diameters to 4.2 m made of Uranus 52 N?
Also, a couple of major Indian suppliers could help you, same Uranus 52 N or even 2507.
Thickness to 5" in Spain.
Caution;- dished end forming of this material would invariably force you to compromise the theoretical shape, so be prepared.