Hey everyone
We have a problem about heat treatment of LCB which we fail in impact result. First I should say that I have read every single related thread in this site.
We have THREE different chemical composition as :
C: 0.22
Si: 0.26
Mn: 0.81
Cr: 0.16
Ni: 0.35
Mo: 0.08
Cu: 0.05
P: 0.01
S: 0.02
Al: 0.046
Sn:0.009
Ti:0.063
-------------------
C: 0.23
Si: 0.26
Mn: 0.90
Cr: 0.14
Ni: 0.32
Mo: 0.092
Cu: 0.04
P: 0.01
S: 0.016
Al: 0.061
Sn: 0.008
Ti: 0.048
-------------------
C: 0.22
Si: 0.3
Mn: 0.99
Cr: 0.14
Ni: 0.34
Mo: 0.09
Cu: 0.04
P: 0.01
S: 0.014
Al: 0.046
Sn: 0.007
Ti: 0.059
we did these cycle for heat treatment and here is the results: (we need impact result of average 18 J)
1. 940 C - 2h - Air Cool; 898 C- 2h - Water quench - 676 6 h quench up to 300C and then normalize. (Partial similar to what suggested here
Impact result: 4 J !!!
UTS: 736!! mpa
2. 940 C - 2h - Air Cool; 898 C- 2h - Water quench - 676 4h quench up to 300C and then normalize
Impact result: 5 J !!!
UTS: 643!! mpa
Soak at 650 C 1 hour; 930 C water quench 2 hour; 590-600 2 hour Air cool
impact result : 17 J
UTS: 627
and this is a 16" valve of LCB.
we didn't reach impact result from what suggested in this forum and other threads. Any idea to get impact result of 18 J ? is soaking time appropriate for a 16" valve?
and please be aware that we have almost no chance to change the chemical composition and should focus on heat treatment.
thank you in advance.
We have a problem about heat treatment of LCB which we fail in impact result. First I should say that I have read every single related thread in this site.
We have THREE different chemical composition as :
C: 0.22
Si: 0.26
Mn: 0.81
Cr: 0.16
Ni: 0.35
Mo: 0.08
Cu: 0.05
P: 0.01
S: 0.02
Al: 0.046
Sn:0.009
Ti:0.063
-------------------
C: 0.23
Si: 0.26
Mn: 0.90
Cr: 0.14
Ni: 0.32
Mo: 0.092
Cu: 0.04
P: 0.01
S: 0.016
Al: 0.061
Sn: 0.008
Ti: 0.048
-------------------
C: 0.22
Si: 0.3
Mn: 0.99
Cr: 0.14
Ni: 0.34
Mo: 0.09
Cu: 0.04
P: 0.01
S: 0.014
Al: 0.046
Sn: 0.007
Ti: 0.059
we did these cycle for heat treatment and here is the results: (we need impact result of average 18 J)
1. 940 C - 2h - Air Cool; 898 C- 2h - Water quench - 676 6 h quench up to 300C and then normalize. (Partial similar to what suggested here
Impact result: 4 J !!!
UTS: 736!! mpa
2. 940 C - 2h - Air Cool; 898 C- 2h - Water quench - 676 4h quench up to 300C and then normalize
Impact result: 5 J !!!
UTS: 643!! mpa
Soak at 650 C 1 hour; 930 C water quench 2 hour; 590-600 2 hour Air cool
impact result : 17 J
UTS: 627
and this is a 16" valve of LCB.
we didn't reach impact result from what suggested in this forum and other threads. Any idea to get impact result of 18 J ? is soaking time appropriate for a 16" valve?
and please be aware that we have almost no chance to change the chemical composition and should focus on heat treatment.
thank you in advance.