TieGuy07
Civil/Environmental
- Jul 10, 2007
- 5
- 0
- 0
I've got a proprosed 6ft wide reinf concrete sidewalk I've been told to beef up (and then some) to ensure that the frequent truck traffic does not break it up. I've been told to use a 10" thick reinf. conc. section. The soils in the area are typically clayey with high PIs (past 20). Given the overkill with the concrete thickness I plan to use a 6-inch thick base of either: lime stabilized subgrade, cement stabilized sand, or crushed aggregate? I'm not sure why picking say cement stabilized sand is better/worse than cr. agg. -don't think lime stab is the way to go with a 6ft width but it's typically used in this locale -help would be appreciated.