looking for some lubricant Mil PRF 3150 in Mexico

Status
Not open for further replies.

lombardo

Petroleum
Jun 8, 2002
27
Im looking for some lubricant that meets this Mil Norm (PRF 3150) somebody know the comercial name of this kind of lubricant in Mobil or Exxon brand? or some alternative easy to find in Mexico that meets this Norm.
Thanks
Alejandro Peterson
 
Replies continue below

Recommended for you

MIL-PRF-3150 Lubricating Oil, Preservative, Medium
QPL:

Sensyn 3150 Sentinel Canada
Tectyl 802A Daubert Chemical Company, Inc.
NOX Rust X-217 "
Brayco 350 Air BP Lubricants
Royco 315 Anderol Inc.
Arpolube 3150 Arpol Petroleum Div., CSD Corp
Coating oil CO-100 United Oil Company
 