hi all

i having an issue with some carbon material which has been bought in as 26kg blends.
these are melted down in a 30kg inverted furnace and cast.
after cast sample analysis is taken,the carbon levels are way below the spec.

bought in charge Carbon = 0.020
cast sample analysis = 0.016

can anyone help please?

thanks

lak
 
Replies continue below

Recommended for you

Did you take into account the oven efficiency value in the load calculation?
If so, maybe you overestimated it.
 
Can you explain what you are doing?

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 