Christo_AU
Structural
- Sep 4, 2023
- 20
Some help please with a newbie question. If I machine a big screw, will it retain it's strength and hardness? Does it have the rated strength and hardness throughout it's thickness or is it softer in the centre?
For example: Using a lathe, I turn down an M20 bolt to have a shoulder with an M10 thread on it. Can I assume the M10 section would retain the rated strength, e.g. grade 8.8?
I am asking this because I am unsure if machining will produce enough heat to remove the hardening/tempering, as is the case with welding. Thank in advance.
For example: Using a lathe, I turn down an M20 bolt to have a shoulder with an M10 thread on it. Can I assume the M10 section would retain the rated strength, e.g. grade 8.8?
I am asking this because I am unsure if machining will produce enough heat to remove the hardening/tempering, as is the case with welding. Thank in advance.