Magnet with gravity force

Status
Not open for further replies.

JustOnePost

Aerospace
Jul 30, 2013
1
Is it possible to create a magnet that pulls with the same force as gravity?
 
Replies continue below

Recommended for you

Exactly?

Gravity is the weakest force of the four fundamental forces.

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529
 
Your post suggests that the force is constant. It isn't. The force experienced depends on the separation distance between the magnet and the object, the electrical and magnetic properties of the object, etc.

Maui

 
It might be possible, but very limiting.
First, you need to figure out the force the magnet creates on a moment, with respect to it's distance.