Mastic for steel column/base plate protection

Status
Not open for further replies.

braves25

Structural
Jan 2, 2004
64
Hello all,

We typically call for the column, base plate, and anchors to be coated with mastic when below grade for corrosion protection. Does anyone know of a good product for this type of application? We generally just leave it up to the contractor, but I am being asked to specify a specific mastic. Any suggestions?
 
Replies continue below

Recommended for you

D.S. Brown has a spray on membrane called Deckguard. Although it's a concrete deck product railroads use it to waterproof ballast plates on thru girder bridges. I know another product but the name escapes me at the moment. When I get home I'll find it. It's a similar product used on railroad bridges.
 
Here's a possible note:

Below_Grade_Coating_Note_fsoez1.jpg


Check out Eng-Tips Forum's Policies here:
faq731-376
 
The other product I mentioned is Eliminator HM by Stirling Lloyd.
 
Avoid tar modified epoxies that can be carcinogenic.

Dik
 