Material for ball bearing at high temperature

Status
Not open for further replies.

davidmoul

Materials
Jun 20, 2008
60
Hello everyone.

Does anyone know a material for a ball bearing that have to support 300°C in service, which would be quite simple to find and supply?

We have specific ball bearing designed, and we would like to change the material to be able to design a machine supporting 300°C. Any idea?

Thank you for your precious help!
 
Replies continue below

Recommended for you

Is it possible to cool the bearings by a suitable jacket around it,so that you could avoid the use of expensive high temperature bearing materials?

Chocolates,men,coffee: are somethings liked better rich!!
(noticed in a coffee shop)
 
You will also need high temp synthetic lubricant. Look on the Kytox web site.
Ceramic bearings, at least ceramic rollers are probably needed for this.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 