Hello,
I have the following problem.
I need to select the proper material between AISI 316 L / AISI 316 L NACE / DUPLEX to be suitable for following working condition:
pH = from 2 to 5
Chloride (Cl-) = less than 500 ppm
Sulfates (SO42-) = less than 13700 ppm
Temperature = 25 - 30 °C
In the above stream, I'm dosing following additive:
- Ozone (O3) = dosing rate 280 g/m3 - Injection concentration 8%
- Hydrogen peroxide (H2O2) = dosing rate of pure product (100% H2O2) 75 mg/L - Injection concentration 35%
Could you please help me to understand which is the most suitable material?
Thanks in advance
I have the following problem.
I need to select the proper material between AISI 316 L / AISI 316 L NACE / DUPLEX to be suitable for following working condition:
pH = from 2 to 5
Chloride (Cl-) = less than 500 ppm
Sulfates (SO42-) = less than 13700 ppm
Temperature = 25 - 30 °C
In the above stream, I'm dosing following additive:
- Ozone (O3) = dosing rate 280 g/m3 - Injection concentration 8%
- Hydrogen peroxide (H2O2) = dosing rate of pure product (100% H2O2) 75 mg/L - Injection concentration 35%
Could you please help me to understand which is the most suitable material?