Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Tek-Tips community for having the most helpful posts in the forums last week. Way to Go!

material to make eraser

Status
Not open for further replies.

ppc3

Materials
Aug 29, 2006
1
0
0
US
Hi , i'm looking to buy a material that pencil eraser is made of. I have injection molding application fot that material.I know that they are using pumice + other additives.I'm only worry about that blend of pumice will damage my screw and barrel.Is there anything that i can use with injection molding process to make final product that would work like a eraser??
 
Replies continue below

Recommended for you

Try this:

SMR L 100
White factice 100
Maglite D 30
Lithopone 100
Barytes 80
Whiting 150
Titanium dioxide 10
Light process oil 30
Zinc oxide 10
Stearic acid 2
Sulfur 6-8
MBTS 1-1.5
DPG 1-2
 