shankerm
Chemical
- Mar 17, 2004
- 20
I'am working on designing a reactor for a process that uses KOH and Hydrazine hydrate upto 200C, highly basic and corrosive solutions.
Hydrazine hydrate is not compatible with metals containing Molebdenum. Thus, SS 316 IS RULED OUT. Any other suggesions, From sources, I've learnt that Nickel rich alloy would be suitable .
Any suggesions ???
Thank you !
Hydrazine hydrate is not compatible with metals containing Molebdenum. Thus, SS 316 IS RULED OUT. Any other suggesions, From sources, I've learnt that Nickel rich alloy would be suitable .
Any suggesions ???
Thank you !