Paulettea
Mechanical
- Sep 28, 2016
- 101
Dear All
I am using PV Elite software to model a pressure vessel based on ASME Sec.VIII Div. 2.
Design pressure: 93 barg
Design temperature: 88 C
Shell/Head material: SA-240 304
Shell ID: 3400 mm
Head type: Hemispherical
The problem is that with these conditions the vessel fails in the hydrotest calculations because the stresses are higher than allowable stress for hydrotest. As a normal procedure I increased the thickness of shell but again the vessel fails in hydrotest this time in the head region. Then after increasing head thickness the failure occurs on the shell and this process goes on.
Then I decided not to model the heads at all. This time the calculations were made on just a cylinder and the hydrotest fails again and by increasing the shell thickness this problem cannot be solved at all.
I think the root of this problem is that by increasing the thickness of the shell, the MAWP of the vessel increases too and this makes the problem like an endless loop.
What can I do to remove this problem?
Warm Regards
I am using PV Elite software to model a pressure vessel based on ASME Sec.VIII Div. 2.
Design pressure: 93 barg
Design temperature: 88 C
Shell/Head material: SA-240 304
Shell ID: 3400 mm
Head type: Hemispherical
The problem is that with these conditions the vessel fails in the hydrotest calculations because the stresses are higher than allowable stress for hydrotest. As a normal procedure I increased the thickness of shell but again the vessel fails in hydrotest this time in the head region. Then after increasing head thickness the failure occurs on the shell and this process goes on.
Then I decided not to model the heads at all. This time the calculations were made on just a cylinder and the hydrotest fails again and by increasing the shell thickness this problem cannot be solved at all.
I think the root of this problem is that by increasing the thickness of the shell, the MAWP of the vessel increases too and this makes the problem like an endless loop.
What can I do to remove this problem?
Warm Regards